ADVANTAGES

Laminated magnet

Reduce motor eddy, improve motor efficiency

70-100 um

InsulationThickness

60-250 ℃

Max Working Temp.

2-40 layers

Insulation Layers

-60-300 ℃

Temp. Resistance of the Magnet Surface Coating

Neutral salt spray resistanced
≥500 hrs ;PCT ≥200 hrs

Corrosion Resistance of the Magnet Coating

(Schematic diagram of eddy current)
(Schematic diagram of thermal simulation)